New nickel-based Höganäs Amperprint® 0233 Haynes® 282® powder enhances the capabilities of Velo3D’s end-to-end solution for customers in oil and gas, aviation, energy, space, and other high-value applications

Velo3D, Inc. (NYSE: VLD), a leading metal additive manufacturing technology company for mission-critical parts, has qualified the nickel-based superalloy powder Amperprint 0233 Haynes 282 for use in its Sapphire family of printers. The powder was produced by Höganäs AB—a world leader in metal powder production—under license from Haynes International, Inc., and is designed for high creep strength, thermal stability, weldability, and fabricability not commonly found in other alloys. The material is ideal for high-temperature structural applications like energy generation, gas turbines, and space launch vehicles to build parts like heat exchangers, combustors, nozzles, combustion liners, rocket engines, and shrouded impellers.

The first Sapphire printer utilizing the Amperprint 0233 Haynes 282 powder will be operated by Duncan Machine Products (DMP), a contract manufacturer based in Duncan, Oklahoma. The system will be the seventh in DMP’s fleet of Velo3D Sapphire printers.

“Our goal at Velo3D is to enable engineers to build the parts they want without compromising on the design or quality,” said Benny Buller, Velo3D CEO and Founder. “Qualifying new powdered metals, like Amperprint 0233 Haynes 282, for use in our end-to-end solution, further expands what’s possible with our additive manufacturing technology. Our partners at Höganäs provide materials of the highest quality, and I look forward to seeing what our customers build using this amazing alloy.”

Powdered nickel-based superalloys, like Amperprint 0233 Haynes 282, are often used to print parts for use in high-temperature applications due to the alloy’s resistance to cracking and its ability to operate at near-melting-point temperatures. This tolerance allows parts printed with the alloy to be used in vacuum, plasma, and other demanding applications. Its high weldability makes the powder ideal for parts in larger systems because of its ability to be welded to other components.

Höganäs specializes in creating powders for additive manufacturing, delivering products with consistent spherical shape, tight control on chemistry, and enhanced flowability. The powders are made using the purest materials with very precise compositions of trace elements that give the metals their unique properties.

“It’s inspiring to see what engineers have been able to build using metal powders from Höganäs and Velo3D’s support-free additive manufacturing process,” said Jerome Stanley, Höganäs Director of Global Sales, Customization Technologies. “The first parts printed using our Amperprint 0233 Haynes 282 powder are impressive, and I believe customers are only scratching the surface of what is possible with this superalloy. The powder, combined with Velo3D’s end-to-end solution metal AM solution, is an extremely effective combination for consolidating parts into monolithic structures to eliminate coefficient of thermal expansion in large, high-performance systems.”

Velo3D is one of the first additive manufacturing technology companies to offer Amperprint 0233 Haynes 282 powder to its customers. Many of Velo3D’s customers use its end-to-end solution to produce parts for use in aviation, energy, oil and gas, space, and other high-performance applications, making the powder a good fit for Velo3D’s portfolio. In addition to Amperprint 0233 Haynes 282 powder, metal powders qualified to be printed with Velo3D’s technology include Hastelloy X®, Inconel 718, aluminum F357, Ti 6Al-4V Grade 5, and several additional materials.
www.velo3d.com

 

comments

Related articles

  • Latest Post

  • Most Read

  • Twitter

Who's Online

We have 8496 guests and no members online

We use cookies on our website. Some of them are essential for the operation of the site, while others help us to improve this site and the user experience (tracking cookies). You can decide for yourself whether you want to allow cookies or not. Please note that if you reject them, you may not be able to use all the functionalities of the site.